EN AC-46000 machining data: cutting speed, feed and carbide grade to start with.

Starting cutting speed in m/min and sfm, feed in mm/rev and ipr, the carbide grade class and the setup by operation for EN AC-46000. The numbers are the published N10 Aluminium alloys (cast) sub-group starting band; the designations are on the cross-reference page.

ISO N · Non-ferrous N10 sub-group m/min + sfm · mm/rev + ipr Free, no signup

Every maker's AI recommends its own tools. Ours compares all makers and shows the published source behind each answer, or tells you it could not verify.

01 · AT A GLANCE

EN AC-46000: group, sub-group and condition

ItemValue
ISO 513 groupN Non-ferrous
Sub-groupN10 Aluminium alloys (cast)
Sub-group hardness / condition75–130 HB
CategoryAluminium (die-cast)
EN / WerkstoffnummerEN AC-46000 (AlSi9Cu3(Fe)) · none listed

Hardness is the range published for the whole N10 Aluminium alloys (cast) sub-group on our material guide; the delivery condition of your EN AC-46000 may sit anywhere inside it or outside it.

NEAREST MATCH, NOT A TWIN

At least one designation of this material is a nearest commonly-cited counterpart, not a same-composition equivalent. The machining values below belong to the sub-group, so confirm the actual alloy and delivery condition on the material certificate.

02 · STARTING CUTTING DATA

Cutting speed and feed for EN AC-46000

ConditionVc m/minVc sfmFeed mm/revFeed ipr
N10 Aluminium alloys (cast), 75–130 HB200–800655–26250.05–0.30.002–.012

Sub-group starting values for carbide inserts, from N10 Aluminium alloys (cast). They describe the whole sub-group and are not tuned to EN AC-46000. sfm and ipr are converted from the metric values (1 m/min = 3.281 sfm, 25.4 mm = 1 in). The published band is per sub-group, not per operation; the table below gives the setup by operation. Convert Vc to spindle speed with the speeds & feeds calculator, and see the speeds & feeds guide for the ISO N group range.

Setup by operation

OperationGeometryCoating familyCoolantFirst check
RoughingSharp, high positive rake, polished flute; good chip evacuationPCD for high-silicon alloys and long runs; polished uncoated or DLC carbide otherwiseCoolant or MQLAbrasive silicon wear: move to PCD for life
FinishingSharp, high positive rake, polished flutePCD or polished uncoated / DLC carbideCoolant or MQLBuilt-up edge or smear: raise feed, flush chips
Interrupted cutSharp positive edge, open chipbreakerPCD or polished carbideCoolant or MQLChip evacuation in cavities
Low rigidity / thin wallKeen positive edge, polished flutePolished uncoated or DLC carbideCoolant or MQLPoor finish at high RPM: raise feed per tooth, not just speed

Setup rows are the selection table of the N10 Aluminium alloys (cast) guide. They carry no speeds, so they do not change the starting band above.

03 · CARBIDE GRADES

Carbide grade class for EN AC-46000

PCD for high-silicon cast alloys (A356, ADC12) and long runs; polished uncoated or DLC carbide for low-silicon or short runs.

The P, M, K, N, S or H number inside a grade range describes what the grade is built for, not the workpiece sub-group number, and the two scales must not be matched to each other. We name no single grade here: none of our published sources ties a named grade to this alloy. Pick by ISO class, then compare what the makers publish on the ISO N grade list and in the grade chart.

04 · DESIGNATIONS

EN AC-46000 in EN, US and JIS terms

EN AC-46000 (AlSi9Cu3(Fe)), US A380 (nearest), JIS ADC10 (nearest). The full table, with the nearest-match flags, is on the EN AC-46000 / A380 cross-reference page.

05 · NOTES

How EN AC-46000 behaves in the cut

The high-volume die-casting alloy: silicon makes it abrasive, so PCD or sharp uncoated carbide earns its keep. Cast skin and porosity decide the first pass.

Cost check · free · brand-neutral

Are you overpaying on your EN AC-46000 inserts? Paste your insert list and get a cost audit in about 30 seconds: cross-brand equivalents at the same ISO application position, and where you are likely overpaying. No signup, no sales call.

Run a free cost audit → Check your whole grade list · free

After the free check: a sourced PDF + XLSX report from about USD 10 (EUR 9) per grade. How buying works

06 · FAQ

Common questions

What cutting speed should I start with for EN AC-46000?

The published starting band for the N10 Aluminium alloys (cast) sub-group is 200–800 m/min (655–2625 sfm) at 0.05–0.30 mm/rev (.002–.012 ipr). It is a starting band for the whole sub-group, not a value tuned to EN AC-46000, so confirm on a sample part and adjust for condition, tool and rigidity.

Which carbide grade should I use for EN AC-46000?

PCD for high-silicon cast alloys (A356, ADC12) and long runs; polished uncoated or DLC carbide for low-silicon or short runs. Pick the grade by ISO class rather than by brand name, then confirm the exact grade for your condition. We name no single grade here because none of our published sources ties a named grade to this alloy.

What is EN AC-46000 called in EN, US and JIS standards?

EN AC-46000 (AlSi9Cu3(Fe)) (no Werkstoffnummer listed); US: A380 (nearest); JIS: ADC10 (nearest). At least one pairing is nearest-by-properties, not a drop-in equivalent: the material certificate decides.