CUTTINGTOOLS / AI
Find equivalents
MACHINING DATA · P HOT-WORK TOOL STEEL

AISI H13 machining data: cutting speed, feed and carbide grade to start with.

Starting cutting speed in m/min and sfm, feed in mm/rev and ipr, the carbide grade class and the setup by operation for AISI H13 (X40CrMoV5-1). The numbers are the published P20 Alloy steel (heat treated) sub-group starting band; the designations are on the cross-reference page.

ISO P · Steel P20 sub-group m/min + sfm · mm/rev + ipr Free, no signup

Every maker's AI recommends its own tools. Ours compares all makers and shows the published source behind each answer, or tells you it could not verify.

01 · AT A GLANCE

AISI H13: group, sub-group and condition

ItemValue
ISO 513 groupP Steel
Sub-groupP20 Alloy steel (heat treated)
Sub-group hardness / condition200–300 HB
CategoryHot-work tool steel
EN / WerkstoffnummerX40CrMoV5-1 · 1.2344

Hardness is the range published for the whole P20 Alloy steel (heat treated) sub-group on our material guide; the delivery condition of your AISI H13 may sit anywhere inside it or outside it.

02 · STARTING CUTTING DATA

Cutting speed and feed for AISI H13

ConditionVc m/minVc sfmFeed mm/revFeed ipr
P20 Alloy steel (heat treated), 200–300 HB150–250490–8200.10–0.40.004–.016

Sub-group starting values for carbide inserts, from P20 Alloy steel (heat treated). They describe the whole sub-group and are not tuned to AISI H13. sfm and ipr are converted from the metric values (1 m/min = 3.281 sfm, 25.4 mm = 1 in). The published band is per sub-group, not per operation; the table below gives the setup by operation. Convert Vc to spindle speed with the speeds & feeds calculator, and see the speeds & feeds guide for the ISO P group range.

Setup by operation

OperationGeometryCoating familyCoolantFirst check
RoughingNegative geometry, economical for roughingCVD-coated carbide with a hard top layer for crater resistanceCheck coolant deliveryCrater wear on the rake face: ease Vc
FinishingPositive geometry for finishingCVD-coated carbideCheck coolant deliveryPlastic deformation: edge too hot, drop Vc and feed
Interrupted cutHoned or chamfered edge for securityCVD-coated carbideCheck coolant deliveryEdge security in interruptions; lower the band as hardness climbs
Low rigidity / thin wallPositive geometry for thin walls and low-rigidity setupsCVD-coated carbideCheck coolant deliveryBuilt-up edge at low speed: raise Vc

Setup rows are the selection table of the P20 Alloy steel (heat treated) guide. They carry no speeds, so they do not change the starting band above.

Same sub-group, same starting band: AISI O1 · AISI O2 · AISI P20 · AISI H11

03 · CARBIDE GRADES

Carbide grade class for AISI H13

CVD-coated carbide for crater resistance. Heat-treated alloy steels like 42CrMo4 / 4140 (≈ 28–34 HRC) reward a hard CVD top layer: roughing around P25–P35, finishing around P10–P20.

The P, M, K, N, S or H number inside a grade range describes what the grade is built for, not the workpiece sub-group number, and the two scales must not be matched to each other. We name no single grade here: none of our published sources ties a named grade to this alloy. Pick by ISO class, then compare what the makers publish on the ISO P grade list and in the grade chart.

04 · DESIGNATIONS

AISI H13 in EN, US and JIS terms

EN X40CrMoV5-1, Werkstoffnummer 1.2344, US AISI H13 (UNS T20813), JIS SKD61. The full table, with the nearest-match flags, is on the H13 / 1.2344 cross-reference page.

05 · NOTES

How X40CrMoV5-1 behaves in the cut

Annealed (~200 HB) it machines like a tough alloy steel. At 44-52 HRC it is H-group work: CBN or ceramic turning, or solid-carbide hard milling at hard-material data.

Cost check · free · brand-neutral

Are you overpaying on your AISI H13 inserts? Paste your insert list and get a cost audit in about 30 seconds: cross-brand equivalents at the same ISO application position, and where you are likely overpaying. No signup, no sales call.

Run a free cost audit → Check your whole grade list · free

After the free check: a sourced PDF + XLSX report from about USD 10 (EUR 9) per grade. How buying works

06 · FAQ

Common questions

What cutting speed should I start with for AISI H13?

The published starting band for the P20 Alloy steel (heat treated) sub-group is 150–250 m/min (490–820 sfm) at 0.10–0.40 mm/rev (.004–.016 ipr). It is a starting band for the whole sub-group, not a value tuned to AISI H13, so confirm on a sample part and adjust for condition, tool and rigidity.

Which carbide grade should I use for AISI H13?

CVD-coated carbide for crater resistance. Heat-treated alloy steels like 42CrMo4 / 4140 (≈ 28–34 HRC) reward a hard CVD top layer: roughing around P25–P35, finishing around P10–P20. Pick the grade by ISO class rather than by brand name, then confirm the exact grade for your condition. We name no single grade here because none of our published sources ties a named grade to this alloy.

What is AISI H13 called in EN, US and JIS standards?

EN X40CrMoV5-1 (Werkstoffnummer 1.2344); US: AISI H13 (UNS T20813); JIS: SKD61. Entries marked nearest are the closest commonly-cited counterpart, not a same-composition equivalent.

NEXT

Starting band found. Now the exact grade.

The advisor compares what the makers publish for your material and operation and shows the source behind each answer, or tells you it could not verify.