X10CrNi18-8 is the same material your supplier may list as AISI 301 or JIS SUS301. This page maps the designations across standards and gives the ISO M-group machining starting point, brand-neutral.
| System | Designation |
|---|---|
| EN (EU) | X10CrNi18-8 |
| Werkstoffnummer | 1.4310 |
| AISI / ASTM / UNS (US) | AISI 301 (UNS S30100) |
| JIS (Japan) | SUS301 |
Compiled from the public standard designation systems (EN 10027, SAE/AISI, ASTM, UNS, JIS). Entries marked “nearest” are the closest commonly-cited counterpart, not a drop-in equivalent. Always verify against the material certificate.
The spring-temper austenitic: work-hardens even faster than 304. Cold-rolled tempers cut with high forces; keep the edge under the skin and never dwell.
| ISO group | Starting Vc (coated carbide, turning) | Feed fn |
|---|---|---|
| M M · Stainless steel | 120–220 m/min · 395–720 sfm | 0.15–0.4 mm/rev · .006–.016 ipr |
Group-level starting range from our speeds & feeds guide; convert to RPM with the speeds & feeds calculator. Condition, subgroup and operation shift the number — the material page has the detail: ISO M · Austenitic stainless (spring).
Related materials: AISI 303 / 1.4305 · AISI 304 / 1.4301 · AISI 304L / 1.4307 · AISI 316 / 1.4401 · AISI 316L / 1.4404 · AISI 316Ti / 1.4571
Are you overpaying on the inserts you run in X10CrNi18-8? Paste your insert list and get a cost audit in about 30 seconds: cross-brand equivalents at the same ISO application position, and where you are likely overpaying. No signup, no sales call.
X10CrNi18-8 (Werkstoffnummer 1.4310) corresponds to AISI 301 (UNS S30100). In JIS terms the counterpart is SUS301.
It is an ISO M-group material, so the starting window is 120–220 m/min · 395–720 sfm at 0.15–0.4 mm/rev · .006–.016 ipr for coated-carbide turning, adjusted for condition and operation. For a grounded, brand-neutral pick — grade, geometry and cutting data across 13 brands — ask the advisor.
They designate the same composition under different systems, but the drawing standard governs: certificates, tolerances and delivery-condition requirements differ between standards even for equivalent chemistry. Substitute only with the certificate in hand.
Knowing the material is half the job; picking the grade and cutting data for the operation is the other half. That is what the advisor does, grounded in catalog data and honest when there is no verified match.